| Product |
MgO (%) (min.) |
Cr2O3 (%) min |
SiO2 (%) (max) |
A.P. (%)max |
C.C.S. hgs/ cm2 mint |
PLC at 1600 °C/ 2 hrs |
RUL Ta °C min |
Thermal Spalling (Air quenching) at 1000 °C |
Application |
| CERA-MAC-I |
60 |
15 |
- |
22 |
400 |
-0.5 |
1600 |
|
For general application |
| CERA-MAV-II |
65 |
10 |
- |
21 |
450 |
+_0.5 |
1600 |
|
A.O.D./V.O.D./LRF |
| CERA-MAV-III |
70 |
8 |
- |
22 |
400 |
+_0.5 |
1600 |
|
Alkali resistant brick for paper & chemical industry |
| CARA-FLEX |
82 |
6 |
<1 |
22 |
500 |
+_0.5 |
1700 |
+100 Cycles |
For cement plant rotary kiln |
| CERA-MAV-D-I |
60 |
12-14 |
1.0 |
18 |
450 |
_0.5 |
1750 |
|
VOD/AOD slag zone, and copper smelter |
| CERA-MAV-D-II |
65 |
12-14 |
2.0 |
18 |
450 |
_0.5 |
1750 |
|
Metal zone of VOD/AOD, bottom,free board |
| CERA-MAV-D-III |
80 |
5-6 |
3.0 |
17 |
450 |
_0.5 |
1750 |
|
BOF lining, VOD/AOD/VAD vessel RH.DH vessels |
| CERA-CM-I |
40 |
18 |
- |
24 |
300 |
_0.5 |
1580 |
|
For general application |
| CERA-CHROME |
- |
40 |
- |
21 |
500 |
+/-0.5 |
1480 |
|
Abrasion resistant quality bricks for hearth of soaking pit & reheating furnace
|