| Product |
Setting |
Sintering tem°C |
Grading (mm) |
MgO (%) (min.) |
Cr2O3 (%)min |
SiO2 (%) (max) |
Application Temp°C |
Application |
| CERA-MG-M |
Ceramic |
1550 |
0-0.5 |
80-85 |
- |
- |
1700 |
For laying of magnesite bricks |
| CERA-RAM-80 |
Ceramic |
1500 |
0.5 |
77-82 |
- |
6.5 |
1650 |
For hot & cold repair of steel furnaces |
| CERA-RAM-80S |
-do- |
1500 |
0.5 |
82-84 |
- |
6.0 |
1700 |
Same as above,but with better properties |
| CERA-FET |
-do- |
1500 |
0.5 |
77-82 |
- |
6.5 |
1700 |
For dry fettling of EAF |
| CERA-RAM-95 |
-do- |
1550 |
0.5 |
92-95 |
- |
2.5 |
1800 |
For BOF tap hole ramming |
| CERA-FILL |
-do- |
- |
0-10 |
80 |
- |
- |
1750 |
EBT filling mass for EAF |
| CERA-RAM-D |
-do- |
- |
0.5 |
90 |
- |
- |
1750 |
Dry ramming mass for EAF bottom |
| CERA-GUN-B |
-do- |
- |
0.5 |
75-80 |
- |
6.5 |
1750 |
For repair of EAF Slag zone |
| CERA-GUN-BS |
-do- |
- |
0.5 |
78-84 |
- |
4.0 |
1750 |
For repair of EAF slag zone & L.D. converter |
| CERA-RAM-C 1 |
-do- |
800 |
0-6 |
70 |
8 |
4.0 |
1750 |
For induction furnace producing SS |
| CERA-RAM-A 1 |
-do- |
800 |
0-6 |
70 |
15 |
4.0 |
1750 |
For induction furnace producing Special Steels |
| CERA-RAM-M-1 |
-do- |
800 |
0.8 |
85 |
- |
- |
1750 |
For induction furnace producing Mild steel & Mn steel |