SR.NO. |
TYPICAL APPLICATION |
COATING TYPE |
MACRO HARDNESS |
COATING FUNCTION |
RECOMMENDED PROCESS |
1 |
AGITATOR / IMPELLER WEAR SHAFT |
SS / Cr2O3 |
35 / 58-70HRc |
FATIGUE WEAR & CORROSION |
A / D / P |
2 |
BALL & GATE VALVES |
Cr2O3 / WC-12 Co |
58 - 70 / 55-58 HRc |
CHEMICAL CORROSION RESISTANCE |
D / P / H |
3 |
COMPRESSOR RODS |
Cr2O3 / WC-12 SCo |
58 - 70 /55- 58HRc |
ABRASIVE WEAR RESISTANCE |
D / P / H |
4 |
IMPELLERS |
Cr2O3 / WC - 12 Co |
58 - 70 / 55 - 58HRc |
FATIGUE & CORROSIVE WEAR RESISTANCE |
D / P / H |
5 |
OIL EXPLOTRATION SHAFTS |
WC - 12 Co |
55 - 58 HRc |
ABRASIVE WEAR RESISTANCE |
D / P / H |
6 |
OIL VAPOURIZERS |
SS / Cr2O3 |
35 / 58 - 70 HRc |
CORROSIVE WEAR RESISTANCE |
D / P / H |
7 |
PUMP SLEEVES |
SS + Cr2O3 |
35 / 58 - 70 HRc |
FATIGUE & CORROSIVE WEAR RESISTANCE |
D / P / H |
8 |
PUMP PLUNGER ROD |
SS + Cr2O3 |
35 / 58 - 70 HRc |
CORROSIVE WEAR RESISTANCE |
D / P / H |
9 |
PLUG VALE |
Cr2O3 |
58 - 70 HRc |
CHEMICAL CORROSION RESISTANCE |
D / P / H |
10 |
PUMP SHAFTS & HOUSING |
Cr2O3 |
58 - 70 HRc |
CORROSIVE WEAR RESISTANCE |
D / P / H |
11 |
SHAFT FOR MIXER |
Cr2O3 |
58 - 70 HRc |
CORROSION & ABRASION RESISTANCE |
D / P / H |
12 |
SLURRY PUMP CASING |
Cr2O3 |
58 - 70 HRc |
CORROSIVE WEAR RESISTANCE |
D / P |
13 |
THERMO WELLS |
WC - 12 Co |
55 - 70 HRc |
HEAT ABUSE & CORROSION RESISTANCE |
D / P |
14 |
TANKS & VESSELS |
SS |
58 - 70 HRc |
CORROSIVE WEAR RESISTANCE |
A / D / P / H / PF |
15 |
WELL CASINGS |
SS, WC - 12 Co |
35,,55-58 HRc |
CORROSIVE WEAR RESISTANCE |
D / P / H |
A : WIRE ARC SPRAY PROCESS |
D : DETONATION SPRAY PROCESS |
P : PLASMA SPRAY PROCESS |
H : HVOF SPRAY PROCESS |
M : METALLIZING-WIRE FLAME SPRAY PROCESS |
PF : POWDER FLAME SPRAY PROCESS |